1、

A kind of vinyl acetate ethylene copolymer emulsion was prepared. With a viscosity range from 3 300 to 4 500 mPa · s.

介绍了一种粘度在3300~4500mPa·s之间的醋酸乙烯-乙烯(VAE)共聚乳液的工艺制备方法。

互联网摘选

2、

This article introduced the whole tap stopper made of particles from fused corundum, scaled graphite, fused zircon mullite and a little of additive and binder under 150 Mpa.

本文介绍了利用电熔刚玉、鳞片状石墨、电熔锆莫来石、少量添加剂与结合剂,分别造粒后于150Mpa压力下一次复合而成整体式塞棒。

互联网摘选

3、

When flow velocity reaches 2.62 m/ s, the local corrosion is pitting corrosion and the protective corrosion product film can not form on the test coupon surface at the temperature of 100 ℃ and the CO_2 pressure of 0.03 MPa.

在流体速度为2.62m/s的情况下,温度为100℃、CO2分压为0.03MPa时,发生的局部腐蚀主要为点蚀,试样表面未能形成保护性腐蚀产物膜;

互联网摘选

4、

The maximum tensile strength of the nanocrystalline copper reached to 590 MPa, about 4.5 times of the one of the coarse crystalline copper. The maximum tensile elongation of the nanocrystalline copper reached 10%.

制备的纳米晶铜最大抗拉强度高达590MPa,是普通粗晶铜的4.5倍,纳米晶铜的最大伸长率为10%。

互联网摘选