Annealing: Heating to 820 ~870 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至820~870℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
One two-speed annealing furnace Glassware, Kao Hua furnace, favored by the industry.
其中双速玻璃制品退火炉 、 烤花炉, 深受同行业青睐.
互联网摘选
Annealing: Heating to 400 ~650 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至400~650℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
In addition, this kind of material could be machined after annealing treatment.
且该材质具有退火后可切削加工的性能.
互联网摘选
In the paper, the structure of morden continuous annealing furnace was introduced.
文章介绍了现代用于冷轧不锈带钢生产的连续退火炉的组成及结构.
互联网摘选
Annealing: Heating to 740 ~770 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至740~770℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
Annealing: Heating to 800 ~880 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至800~880℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
The microstructures of Cu-Zn powder under different annealing conditions were studied.
研究了铜锌粉末在不同退火工艺下的显微组织变化.
互联网摘选
Annealing: Heating to 710 ~740 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至710~740℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
Braising , boiling, annealing, setbacks and struggling all necessary processes of shaping.
炖 、 熬 、 磨练 、 挫折、挣扎,这些都是成长必经的过程.
互联网摘选
Hard elastic polypropylene is formed by crystallized under strain and annealing.
硬弹性聚丙烯是在应变结晶和热结晶两个复合过程中形成的.
互联网摘选
Annealing: Heating to 780 ~820 Holding time 1 ~3 h, Colding in furnace.
退火: 加热至780~820℃,在此温度停留1~3小时, 在炉中冷却.
互联网摘选
To optimize sub-job assignments, two simplified algorithms of simulated annealing are proposed.
为优化子作业指派, 提出了两个简化的仿真退火算法.
互联网摘选
随退火时间的延长,α-Fe(Si)的体积分数,Si含量及DO3有序区尺寸增加。
互联网摘选
Study on Strip Breakage Inside Furnace of Continuous Annealing Line of Cold Rolled Sheet
冷轧薄板连续退火线炉内断带原因分析
互联网摘选
本文讨论了高速双极器件制造中的离子注入技术。重点讨论在双极器件制造工艺中的离子注入掺杂技术,离子注入形成浅结技术,以及离子注入层的退火技术。
互联网摘选
武钢硅钢厂退火生产线经常发生因带钢跑偏造成断带事故。
互联网摘选